Brick Veneer Siding in New Jersey by Tri-State Roofing and Chimneys

Brick Veneer Siding in New Jersey: Repair and New Brick Walls

Brick veneer repair and installation: flashing, weeps, lintels and ties.

About Our Brick Veneer Siding Service

Brick veneer, the brick siding on many post-war New Jersey houses, is one layer of real brick tied to the wall behind it, with an air gap between them and flashing and weep holes at the bottom to let water out. When it fails, the drainage path is usually why: weeps buried or caulked shut, flashing that rusted or was never installed, a steel lintel rusting over a window, or a roof edge emptying into the wall. We repair brick veneer across New Jersey and handle new brick veneer installation on additions and new homes. Estimates are free and written.

Which Kind of Brick Siding Is on Your House?

Many post-war brick-front houses in North Jersey have anchored brick veneer, but four other systems also get called brick siding, and each is repaired differently:

  • Solid brick: load-bearing walls two or more bricks thick, found on many pre-war houses and older multi-family buildings.
  • Anchored brick veneer: one layer of brick, an air space and a backup wall (usually wood framing, sometimes block), joined by metal ties.
  • Thin brick: slices of brick, most 1/2 to 1 inch thick, bonded to the wall.
  • Brick-look panels: manufactured siding, not masonry.
  • Brickface: a cement or stucco coat tooled to look like brick.

Weep holes, small gaps or tubes in the bottom course and above windows, usually mean veneer or a cavity wall; end-on bricks in regular rows only hint at solid brick. The surest check is the back of the wall, often visible in an unfinished garage: wood studs mean veneer on a frame wall; concrete block can mean veneer over block or a solid brick-and-block wall with no air space, so check for an air space or existing weeps before anyone drills; brick behind brick means solid masonry. Drilling weeps into solid brick, or cutting joints out of brickface, are expensive mistakes.

This page covers the veneer wall itself: ties, flashing, weeps, lintels and new brick veneer. Repointing, steps and stoops are on our masonry and repointing page, and vinyl or panel siding is covered under siding repair.

How Does a Brick Veneer Wall Keep Water Out?

A brick veneer wall keeps water out by draining it, not by stopping it at the brick. The Brick Industry Association (BIA) classifies it as a drainage wall: rain soaks in, a nor'easter drives some through, and that water runs down the back of the brick and out. An air space, nominally 1 inch with standard ties, lets it fall clear, a water-resistive barrier on the sheathing stops what crosses, and flashing at the base and at lintels turns it out through weep holes just above.

Metal ties hold the brick across the air space. Under the 2024 International Residential Code (IRC) as adopted in New Jersey, in force since August 17, 2026 (a complete permit application submitted by February 17, 2027 may still be reviewed under the previous code), ties are corrosion-resistant and each generally carries no more than 2.67 square feet of wall (2 square feet where design wind pressure exceeds 30 psf), at most 32 inches apart horizontally and 24 vertically.

BIA asks for more than the code minimum:

  • Weeps no more than 24 inches apart, not the code's 33.
  • Flashing run past the brick face as a drip, so water falls clear.
  • Flashing and weeps at every break in the air space, including window and door heads and sills, roof-to-wall intersections, and porch, deck or stair attachments.
  • A clear cavity. The code permits mortar in the air space and even grout fill, but BIA and the International Institute of Building Enclosure Consultants (IIBEC) prefer it clean, since wet mortar against the sheathing wrap carries water inward.

What Goes Wrong With Brick Veneer in New Jersey

Most brick veneer failures in New Jersey trace back to water held in the wall. The common ones:

  • Blocked weeps: mulch over the bottom course, mortar droppings in the cavity, or weeps caulked against insects. Signs: white efflorescence at the base, a wet basement rim joist.
  • Freeze-thaw spalling: brick kept wet by an overflowing gutter, a downspout or a stoop freezes and its face pops off. Wrong-grade brick or a hard repoint on soft older brick speeds it up.
  • Rusting steel lintels: rust takes up more room than steel, so the lintel over a window or garage door lifts the brick. Signs: flaking rust, stair-step cracks from its ends, later a sag.
  • Missing kick-out flashing: where a porch or garage roof eave meets brick, the code requires flashing that diverts water away. Without it, the roof empties into the wall.
  • Sealers, paint and sandblasting: film-forming sealers and non-breathable paint stop the brick drying, so trapped water freezes and pops the face. Sandblasting strips old brick's hard fired surface.
  • Bulging: corroded or missing ties, or foundation movement. Signs: the wall bows when you sight along it, or a gap opens at the window trim.

Should Brick Veneer Be Repaired, Re-Anchored or Rebuilt?

Isolated spalled bricks and blocked weeps are repairs, failed ties mean re-anchoring or re-laying that section, and BIA's structural warning signs (below) generally call for an engineer's assessment. The standard fixes, from BIA's maintenance guidance and the code:

  • Isolated spalled bricks: fix whatever keeps that spot wet, then replace the units with the closest available match, judged against your weathered wall in daylight, the same way we match brick on chimney rebuilds. Nobody can promise an exact match on old brick.
  • Blocked weeps: probe them clear with a thin dowel or stiff wire, or drill new ones with a depth stop to spare the flashing. Drilled weeps only work with flashing behind them; otherwise the fix is the flashing.
  • Failed base flashing: remove brick in alternating 2- to 5-foot sections, lap new flashing at least 6 inches, and let rebuilt sections cure 5 to 7 days before opening the ones between, or brace longer runs temporarily.
  • Rusted lintel: shore the brick, remove it and the old lintel, set a noncombustible lintel (steel shop-coated against rust or made corrosion-resistant) with the code's minimum 4 inches of bearing each end, flash it, re-lay the brick.
  • Tie failure: retrofit anchors tested in a mock-up on your wall, or re-lay the section with new ties.
  • Failed caulk at windows: backer rod and elastomeric sealant, never mortar.

BIA lists structural signs that generally warrant a professional engineer: cracks wider than about 2 mm (0.075 inch), roughly the thickness of a nickel; cracks through several bricks; stepped or diagonal cracking; widespread spalling; rust built up on lintels; brick bowing out of plane; and sills that are flat or slope back toward the house. Repointing over these hides the movement. If the foundation moved, fix that first with foundation repair.

Brick Veneer Installation: Full Brick, Thin Brick or Brick-Look Panels?

Choose full brick where the wall can get a foundation ledge or a code-prescribed steel angle, thin brick where it can't, and brick-look panels only if you want the look without masonry. Full brick veneer is real brick, a nominal 3 or 4 inches thick, over a drainage cavity. Thin brick is bonded to the wall with mortar or adhesive and needs no ledge. Brick-look panels are siding, not masonry.

On a one- to three-story wood-framed house, New Jersey's code lets veneer up to 5 inches thick and 50 pounds per square foot rise 30 feet above a noncombustible foundation, plus 8 feet at a gable. Above a porch roof, the code also lets brick bear on a steel angle at least 6 by 4 by 5/16 inch, lagged into doubled studs or set on the roof framing, bearing on at least two-thirds of the brick's width, with no more than 12 feet 8 inches of brick above it. It is a code-prescribed detail, not a bracket on the siding: the framing must be stiff enough to meet the code's deflection limit, and a vertical movement joint separates that brick from brick on the foundation.

On an existing frame wall, full brick adds about 4 to 5 inches (a nominal 3- or 4-inch brick plus the air space), so jambs, sills, soffits and trim need extending, and every opening needs a lintel. On a new home or addition, the ledge goes into the foundation from the start; see new construction exteriors. For full brick, ask for Grade SW (severe weathering): BIA recommends it where weathering is severe, it is the default grade under ASTM C216, and BIA names the wrong brick choice as a cause of spalling.

Thin brick suits accent walls and partial fronts. BIA notes it generally beats lightweight claddings on impact, fire and sound. The code requires a water-resistive barrier and a means of drainage behind it (BIA prefers a drainage mat), 4 inches of clearance above soil or 2 above paving, and a screed or flashing at the foundation.

Panels are maintained like any siding, and brickface like stucco. If a wall can't carry full brick, the real choice is thin brick, brick-look panels, or plain vinyl siding.

What Does a Good Brick Veneer Job Look Like?

From the yard, a good brick veneer job shows open weeps above the flashing, a flashing edge at the base, a bottom course clear of mulch, sealant rather than mortar at window frames, sills sloped outward, and kick-out flashing where a roof eave meets the brick.

During the work, the cavity stays clear of droppings, and old mortar comes out with a shrouded grinder on a dust collector plus respirators, the setup OSHA's silica standard lists. Red flags: "we'll seal it so it won't leak", skipped weeps, brick laid on a slab edge with no flashing, and a hard cement-rich repoint on soft pre-war brick.

Questions to ask any mason before you sign:

  • Where will the flashing and weeps be?
  • Are you replacing flashing or only clearing weeps, and why is that enough?
  • If you find rusted ties or a failed lintel, how does the scope change, and who decides on an engineer?
  • Will you show me brick and mortar samples against my wall, in daylight?
  • Is a permit being pulled, and does the contract say so?
  • If the house was built before 1978, can I see your EPA RRP firm certificate?

On a house built before 1978, EPA's Renovation, Repair and Painting rule requires an EPA-certified firm and lead-safe practices for paid exterior work that disturbs more than 20 square feet of painted brick or trim, and at any size for demolition of painted surfaces or for work that runs power grinders, sanders or similar machines over paint (allowed only with shrouds and HEPA vacuum attachments; open-flame paint removal is banned outright). We're an EPA Lead-Safe Certified firm with a certified renovator on our team, and you're welcome to see our EPA RRP firm certificate before work starts.

When Not to Seal, Repoint or Add Brick

Skip the brick work when the real problem is water or support the brick can't fix:

  • Don't seal or paint brick to stop a leak. BIA says repellents aren't necessary on properly built brick or recommended on new veneer, and film-forming coatings shouldn't go on brick in freeze-thaw environments.
  • Don't repoint a bulging wall. The ties or the support are the problem.
  • Don't put thin brick over a wall that is already wet or rotted.
  • Don't add brick to a wall soaked by roof runoff or bad grading until the gutters, kick-outs and grade are fixed.
  • Don't add full brick without a bearing plan. If the ledge or steel angle costs more than the look is worth to you, vinyl siding needs no new support.

Permits and Contracts in New Jersey

Whether brick veneer work needs a permit depends on what it touches, and your town's construction official decides. Under N.J.A.C. 5:23-2.7, repairing or replacing existing siding (other than polypropylene) on a one- or two-family house is ordinary maintenance with no permit, but that list doesn't mention brick or masonry, so the official decides how brick repair is treated. Work affecting structural safety or a bearing support is not ordinary maintenance, so expect new veneer on a ledge, lintel replacement or rebuilding a bulged section to need a permit (some of it may qualify as minor work).

New Jersey law (N.J.S.A. 56:8-151) requires a signed, written contract for home improvement work above a small statutory dollar threshold, which covers almost any brick veneer job. It must include the contractor's registration number, a copy of their liability insurance certificate and the insurer's phone number, and the total price including finance charges. You can cancel for any reason before midnight of the third business day after receiving your copy. Our NJ HIC registration number is 13VH12696700; see our credentials.

If a storm or falling limb damaged the wall, we document the damage in writing and photos for your own claim. In New Jersey, only a licensed public adjuster may negotiate a claim on your behalf; see insurance claims.

What Drives the Scope of the Job

We don't publish prices; what a brick wall costs to fix is set by what failed behind it. A free written estimate weighs these variables, and financing is available and explained at the estimate:

  • Repair, re-anchor or rebuild.
  • Feet of flashing, and the number and span of lintels.
  • How hard the brick is to match.
  • Full veneer, thin brick or panels, and any ledge or steel-angle work.
  • Access to second-story walls and gables.
  • Whether an engineer and a permit are involved.
  • Season, since masonry isn't laid in freezing weather without protection.

Why the Roof and the Brick Should Be One Crew's Job

Where a roof meets a brick wall, the flashing belongs to both trades, and a leak that shows up below the brick can start there. On a brick wall, the roofer's step flashing should be covered by counterflashing set into a cut mortar joint. Split between two contractors, it can end up as metal caulked to the brick face, which is only as good as the caulk. Our crew handles roofing, chimneys, masonry, siding and gutters, so that detail is built once and one contractor answers for it. If water shows up inside below a roof-to-wall line, start with roof leak repair.

What's Included

  • Diagnosis of leaks, spalling, cracks and bulges in brick walls
  • Spalled brick cut out and replaced with the closest available match
  • Blocked weeps and failed flashing traced, with the fix in writing
  • Cracks over windows checked for rusting lintels before any patching
  • New brick veneer on additions and new homes
  • Kick-out and roof-to-wall flashing built by the same crew

Brick Veneer Siding — Common Questions

Is brick siding the same as brick veneer?

Brick siding and brick veneer are not always the same thing, because "brick siding" gets used for five different systems: solid load-bearing brick, anchored brick veneer, adhered thin brick, brick-look panels, and brickface, a cement coat tooled to look like brick. On many post-war North Jersey houses with a brick front, it is anchored veneer: one layer of real brick, an air gap, and a backup wall, usually wood framing, held together with metal ties. Weep holes along the bottom course point to veneer. Rows of end-on bricks hint at solid masonry. A continuous cement coat with tooled joints is brickface.

What are the small holes at the bottom of my brick wall, and should I fill them?

The small holes at the bottom of a brick wall are weep holes, and you should never fill them. They let water that gets behind the brick drain out over the flashing. The residential code requires them directly above the flashing, no more than 33 inches apart and at least 3/16 inch across, and the Brick Industry Association recommends no more than 24 inches apart. Caulking them, mortaring them or stuffing them with steel wool traps water against the sheathing and framing. If insects are the concern, noncorrosive weep screens keep the opening draining while keeping pests out.

Why is my brick veneer cracking above the windows?

Stair-step cracks above a window or garage door often come from a rusting steel lintel, the angle that carries the brick over the opening. Rust takes up more room than steel, so it lifts the brick and lets the lintel sag, and it is often mistaken for settlement. The Brick Industry Association treats stepped cracking and rust on lintels as structural signs that generally warrant an engineer's look, not a mortar patch. The usual fix, once the cause is confirmed, is shoring the brick above, removing it and the old lintel, setting a new lintel with flashing, and re-laying the brick, reusing sound originals and matching the rest as closely as the brick allows. Replacing a lintel is structural work, so expect your town's construction official to require a permit.

My brick wall is bulging or pulling away from the house. Can it be fixed without tearing it down?

Bulging brick veneer can sometimes be fixed without tearing it down, depending on how far it has moved. Bulging usually means the ties holding the brick to the frame have corroded or were never installed, or the support under the brick has moved. Keep people away from any section that is visibly loose and get it assessed, since out-of-plane movement is on the Brick Industry Association's list of structural warning signs. The fix is either retrofit anchors, tested on your wall in a mock-up first, or taking the section down and re-laying it with new ties and flashing. Repointing a bulged wall only hides the movement.

Should I seal my brick to stop leaks?

Sealing brick usually won't stop a leak, because brick veneer is designed to get wet and drain. Leaks usually come from failed flashing, blocked weeps, open joints or roof-to-wall details, and a sealer fixes none of those. The Brick Industry Association says water repellents aren't necessary on properly built brick and aren't recommended on new veneer, and that film-forming coatings shouldn't be used on brick in freeze-thaw environments, because they stop the wall drying and can cause spalling. Find and fix the water path first.

Can a brick front be added to a house that has vinyl siding?

A brick front can be added to many vinyl-sided houses, as long as the brick has a foundation ledge or a code-prescribed steel angle to bear on, never the existing siding or sheathing. The wall gets about 4 to 5 inches thicker, so window and door jambs, sills, soffits and trim need extending, and every opening needs a lintel. Thin brick avoids the ledge but is a different system, adhered to the wall with a drainage layer behind it. Because full brick adds structural load, expect a permit conversation with your town's construction official.

Thin brick or full brick veneer: which holds up better in New Jersey?

Neither wins by default: full brick veneer has a drainage cavity built into the wall, while thin brick holds up only as well as the drainage layer installed behind it. Thin brick is a slice, most of it 1/2 to 1 inch thick, bonded to the wall. It makes sense where full brick can't be supported, such as accent walls and partial fronts, and the Brick Industry Association notes it generally beats lightweight claddings on impact and fire. It needs a means of drainage behind it (the Brick Industry Association prefers a drainage mat), clearance above soil and paving, and a screed or flashing at the foundation. For full brick, ask for Grade SW.

Do I need a permit for brick veneer repair in NJ?

It depends on the work, and your town's construction official decides. Siding repair on a one- or two-family house is ordinary maintenance under N.J.A.C. 5:23-2.7, but that rule doesn't mention brick, and structural work such as lintel replacement, rebuilding a bulged section or new veneer on a ledge falls outside it, so ask the contractor to state the permit status in the written contract.